Moulin Fritte M85

Description: Fritte boro-alcaline

Oxide Analysis Formula Tolerance
B2O3 37.00% 4.71
Na2O 7.00% 1.00
SiO2 56.00% 8.25
Oxide Weight 885.71
Formula Weight 885.71

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 505C