Description: Fritte boro-alcaline
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 16.07% | 1.00 | |
| B2O3 | 36.43% | 2.02 | |
| SiO2 | 47.50% | 3.05 | |
| Oxide Weight | 385.81 | ||
| Formula Weight | 385.81 | ||
Corrected chemistry Oct 2022, it was:
Na2O 15.0, Al2O3 51.0, SiO2 34.0
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 548C |
|---|
| By Tony Hansen Follow me on ![]() | ![]() |