Alternate Names: Fritte M 1511
Description: Fritte Boro-acaline Plombeuse
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 36.90% | 0.50 | |
| B2O3 | 23.10% | 1.01 | |
| Na2O | 10.20% | 0.50 | |
| SiO2 | 29.80% | 1.50 | |
| Oxide Weight | 303.18 | ||
| Formula Weight | 303.18 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 504C |
|---|