1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Glasurfritten 35.32

Alternate Names: 35 32,35-32

Description: Blei-Bor-Silikat-Fritte

Oxide Analysis Formula Tolerance
PbO 68.57% 1.00
B2O3 19.80% 0.93
SiO2 11.63% 0.63
Oxide Weight 325.51
Formula Weight 325.51

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 75 x 10-7
Frit Softening Point 473C
Frit Melting Range (C) 800-1080C