Alternate Names: 35 2,35-2
Description: Bleihaltige Zinkmatt-Fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 23.00% | 0.19 | |
| CaO | 5.00% | 0.16 | |
| Na2O | 2.00% | 0.06 | |
| ZnO | 27.00% | 0.60 | |
| B2O3 | 4.00% | 0.10 | |
| Al2O3 | 2.00% | 0.04 | |
| SiO2 | 37.00% | 1.11 | |
| Oxide Weight | 179.82 | ||
| Formula Weight | 179.82 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 61 x 10-7 |
|---|---|
| Frit Softening Point | 600C |
| Frit Melting Range (C) | 970-1030C |