Alternate Names: 34 41,34-41
Description: Blei-Aluminium-Silikat-Fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 74.56% | 1.00 | |
| Al2O3 | 4.78% | 0.14 | |
| SiO2 | 20.66% | 1.03 | |
| Oxide Weight | 299.36 | ||
| Formula Weight | 299.36 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 77 x 10-7 |
|---|---|
| Frit Softening Point | 500C |
| Frit Melting Range (C) | 900-1080C |