Alternate Names: Frit 21 C003
Description: Fritte Boracique
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 5.43% | 0.40 | |
| CaO | 3.69% | 0.30 | |
| MgO | 2.21% | 0.25 | |
| ZnO | 0.89% | 0.05 | |
| Al2O3 | 6.70% | 0.30 | |
| B2O3 | 15.25% | 1.00 | |
| SiO2 | 65.83% | 5.00 | |
| Oxide Weight | 456.35 | ||
| Formula Weight | 456.35 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Melting Range (C) | 1030-1180C |
|---|