Ferro Frit 3271

Oxide Analysis Formula Tolerance
SiO2 54.58% 2.25
B2O3 21.54% 0.77
Na2O 12.87% 0.51
CaO 11.01% 0.49
Oxide Weight 247.62
Formula Weight 247.62

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.3 x 10-6 (50-450C)
Frit Melting Range (C) 1500F