Frit VO 6147

Description: Reimbold & Strick fast firing Zn,Ca matte frit

Oxide Analysis Formula Tolerance
Al2O3 13.00% 0.22
Na2O 6.00% 0.16
SiO2 47.00% 1.32
CaO 14.00% 0.42
ZnO 20.00% 0.42
Oxide Weight 168.91
Formula Weight 168.91

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 73 x 10-7 (20-400C)
Frit Softening Point >800C