Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit VO 6104

Description: Reimbold & Strick calcium matte frit

Oxide Analysis Formula Tolerance
B2O3 10.00% 0.25
CaO 30.00% 0.92
SiO2 54.00% 1.54
Na2O 3.00% 0.08
Al2O3 3.00% 0.05
Oxide Weight 171.48
Formula Weight 171.48

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 80 x 10-7 (20-400C)
Frit Softening Point >800C
Glass Transition Temperature 602C
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved