Ferro Frit 1081

Description: Insoluble colemanite substitute

Oxide Analysis Formula Tolerance
CaO 27.05% 1.00
B2O3 50.35% 1.50
Al2O3 4.92% 0.10
SiO2 17.68% 0.61
Oxide Weight 207.39
Formula Weight 207.39

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron).
Materials Ferro Frit 2244
Materials Ferro Frit 2954
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1050-1160C