Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit A 62

Description: Reimbold & Strick stoneware frit

Oxide Analysis Formula Tolerance
B2O3 13.00% 0.60
Na2O 2.00% 0.10
Al2O3 6.00% 0.19
CaO 7.00% 0.40
PbO 34.00% 0.49
SiO2 38.00% 2.04
Oxide Weight 323.24
Formula Weight 323.24

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 66 x 10-7 (20-400C)
Frit Softening Point 610C
Glass Transition Temperature 560C
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy