Frit A 3334

Description: Reimbold & Strick lead borosilicate frit

Oxide Analysis Formula Tolerance
PbO 55.00% 1.00
SiO2 28.00% 1.89
B2O3 17.00% 0.99
Oxide Weight 405.82
Formula Weight 405.82

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 59 x 10-7 (20-400C)
Frit Softening Point 510C
Glass Transition Temperature 480C