Ferro Frit CM-942

Notes

Red leadless cadmium, underglaze mix complete by itself.
Works well with CM-943 to produce oranges. Cone 06.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Available from Laguna Clays
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 1750F
By Tony Hansen