National Premium WT Bentonite

Description: 200 mesh Sodium Bentonite

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying.
Materials HPM-20 Volclay Bentonite
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
URLs https://www.bentonite.com/en/home
BPM Bentonite information