Degussa Frit 90158

Alternate Names: 90158 Natriumborsilikat

Description: Natriubor-Silikat

Oxide Analysis Formula Tolerance
Na2O 16.25% 1.00
B2O3 36.49% 2.00
SiO2 47.26% 3.00
Oxide Weight 381.54
Formula Weight 381.54

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 85 X 10-7 (20-400C)
Heating Microscope Analysis for Frits 514C
Heating Microscope Analysis for Frits 685C
Heating Microscope Analysis for Frits 780C