Degussa Frit 90328

Oxide Analysis Formula Tolerance
MgO 0.35% 0.10
CaO 0.24% 0.05
Na2O 4.52% 0.85
Al2O3 7.88% 0.90
SiO2 65.51% 12.69
B2O3 21.50% 3.60
Oxide Weight 1,164.60
Formula Weight 1,164.60

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 48 X 10-7 (20-400C)
Heating Microscope Analysis for Frits 495C
Heating Microscope Analysis for Frits 795C
Heating Microscope Analysis for Frits 1270C
By Tony Hansen