1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Degussa Frit 90155

Alternate Names: 90155 Alkalizinkborfritte

Description: Alkalizinkoor-fritte

Oxide Analysis Formula Tolerance
CaO 10.73% 0.40
ZnO 15.56% 0.40
SiO2 48.83% 1.70
Na2O 5.93% 0.20
Al2O3 7.31% 0.15
B2O3 11.64% 0.35
Oxide Weight 209.18
Formula Weight 209.18

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 69 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 548C
Heating Microscope Analysis for Frits 770C
Heating Microscope Analysis for Frits 890C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy