Alternate Names: 90142 Calziumboratfritte
Description: Calziumborat-fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 25.71% | 1.00 | |
| SiO2 | 33.05% | 1.20 | |
| B2O3 | 31.89% | 1.00 | |
| Al2O3 | 9.35% | 0.20 | |
| Oxide Weight | 218.20 | ||
| Formula Weight | 218.20 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 66 x 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 632C |
| Heating Microscope Analysis for Frits | 900C |
| Heating Microscope Analysis for Frits | 960C |