Alternate Names: 90062 Bleiborsilikat
Description: Bleiborsilikat
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 62.41% | 1.00 | |
| SiO2 | 8.40% | 0.50 | |
| B2O3 | 29.19% | 1.50 | |
| Oxide Weight | 357.63 | ||
| Formula Weight | 357.63 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 79 x 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 440C |
| Heating Microscope Analysis for Frits | 550C |
| Heating Microscope Analysis for Frits | 640C |