Ceradel Frit 3195

Alternate Names: Ceradel Fritte 3195

Description: Low temperature glaze

Oxide Analysis Formula Tolerance
Na2O 6.00% 0.33
CaO 11.00% 0.67
B2O3 22.50% 1.10
Al2O3 12.00% 0.40
SiO2 48.50% 2.76
Oxide Weight 341.47
Formula Weight 341.47

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Ferro Frit 3195
A commonly used boron frit, it is a balanced glaze all along at cone 06-02 (with the addition of 10-15% kaolin). Not fully glossy.

Data

Co-efficient of Linear Expansion 71.6 (10-7/C 20/300C)
Frit Melting Range (C) 1000-1300C
By Tony Hansen