Ceradel Frit 3134

Alternate Names: Ceradel Fritte 3134

Description: High calcia borosilicate frit

Oxide Analysis Formula Tolerance
Na2O 10.00% 0.31
CaO 20.00% 0.69
B2O3 23.00% 0.64
SiO2 47.00% 1.51
Oxide Weight 193.13
Formula Weight 193.13

Notes

From the name it might be assumed this is a replica of Ferro frit 3134, but Ceradel is providing a slightly different chemistry.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry.

Data

Co-efficient of Linear Expansion 94.7 (10-7/C 20/300C)
Frit Melting Range (C) 1000-1300C
By Tony Hansen