1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Ceradel Frit C 1254

Alternate Names: Fritte C1254, Fritte C 1254, Ceradel Frit 1254

Description: Fritte calco-alcaline sans plomb

Oxide Analysis Formula Tolerance
Al2O3 7.38% 0.20
B2O3 27.73% 1.10
Na2O 11.22% 0.50
CaO 10.15% 0.50
SiO2 43.51% 2.00
Oxide Weight 276.30
Formula Weight 276.30

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 72x10-7 (20/300C)
Frit Softening Point 800-920C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy