Silica Sierra Cristal (Cuba)

Description: Cuban silica

Oxide Analysis Formula Tolerance
Al2O3 0.10% 0.16
MgO 0.06% 0.25
CaO 0.25% 0.75
SiO2 99.16% 277.52
Fe2O3 0.02% 0.02
LOI 0.18%n/a
Oxide Weight 16,751.44
Formula Weight 16,781.64

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.