1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Silica D/Golpe (Cuba)

Description: Cuban silica

Oxide Analysis Formula Tolerance
SiO2 91.00% 30.45
Al2O3 4.00% 0.79
CaO 2.40% 0.86
MgO 0.28% 0.14
Fe2O3 1.00% 0.13
LOI 0.86%n/a
Oxide Weight 1,984.37
Formula Weight 2,001.58

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.
Materials Silica Sierra Cristal (Cuba)