Degussa Frit 90368

Alternate Names: Frit D-90368, Erdalkaliborsilikat D 90368

Oxide Analysis Formula Tolerance
MgO 1.87% 0.10
CaO 18.24% 0.70
Na2O 5.76% 0.20
Al2O3 11.84% 0.25
SiO2 55.82% 2.00
B2O3 6.46% 0.20
Oxide Weight 215.29
Formula Weight 215.29

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 76 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 630C
Heating Microscope Analysis for Frits 830C
Heating Microscope Analysis for Frits 1080C