Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Alkaliborsilikat F 37025

Alternate Names: Frit F-37025

Oxide Analysis Formula Tolerance
SiO2 59.13% 3.00
Na2O 20.33% 1.00
B2O3 20.54% 0.90
Oxide Weight 304.97
Formula Weight 304.97

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 503C
By Tony Hansen