| Monthly Tech-Tip | No tracking! No ads! |
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.14% | 0.01 | |
| Al2O3 | 39.36% | 1.00 | |
| SiO2 | 46.27% | 2.00 | |
| Fe2O3 | 0.74% | 0.01 | |
| LOI | 13.00% | n/a | |
| Oxide Weight | 224.19 | ||
| Formula Weight | 257.69 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Typecodes |
Materials used in Denmark
|