Potclays Frit 2269

Description: This is actually Ferro Frit 3195

Oxide Analysis Formula Tolerance
CaO 11.20% 0.67
Na2O 5.99% 0.33
Al2O3 12.39% 0.41
B2O3 22.99% 1.11
SiO2 47.44% 2.66
Oxide Weight 337.58
Formula Weight 337.58

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3195
A commonly used boron frit, it is a balanced glaze all along at cone 06-02 (with the addition of 10-15% kaolin). Not fully glossy.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.