PotteryCrafts Frit P3134

Alternate Names: PotteryCrafts Frit 3134

Description: This is actually Ferro Frit 3134

Oxide Analysis Formula Tolerance
CaO 20.10% 0.68
Na2O 10.30% 0.32
B2O3 23.10% 0.63
SiO2 46.50% 1.48
Oxide Weight 190.69
Formula Weight 190.69

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.6
Frit Melting Range (C) 980-1000C