Chrysanthos Frit FR005

Description: High boron sodium frit

Oxide Analysis Formula Tolerance
SiO2 65.45% 6.37
Na2O 10.60% 1.00
B2O3 23.95% 2.01
Oxide Weight 584.91
Formula Weight 584.91

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 980-1080C