Chrysanthos Frit FR004

Description: Alumina lead bisilicate frit

Oxide Analysis Formula Tolerance
SiO2 32.96% 1.92
PbO 63.89% 1.00
Al2O3 3.25% 0.11
Oxide Weight 349.70
Formula Weight 349.70

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 79
Frit Melting Range (C) 850-900C
Glass Transition Temperature 552C