Ferro Frit 9146

Alternate Names: Frit DA9146

Description: Dense zircon white frit leadless frit

Oxide Analysis Formula Tolerance
CaO 6.00% 0.46
MgO 0.60% 0.06
Na2O 6.00% 0.42
ZnO 1.10% 0.06
Al2O3 4.10% 0.17
B2O3 13.53% 0.84
SiO2 56.45% 4.05
ZrO2 12.23% 0.43
Oxide Weight 430.84
Formula Weight 430.84

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3302-D
Materials Ferro Frit 1085
Materials Ferro Frit 9102
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 573C
Frit Melting Range (C) 1040-1100C
Glass Transition Temperature 628C