Description: Super white burning kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| TiO2 | 0.09% | - | |
| Al2O3 | 35.50% | 1.00 | |
| SiO2 | 49.50% | 2.37 | |
| Fe2O3 | 0.29% | 0.01 | |
| LOI | 13.80% | n/a | |
| Oxide Weight | 245.32 | ||
| Formula Weight | 284.59 | ||