Alternate Names: Tungsten(IV) Sulfide
Formula: WS2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| WO3 | 93.47% | 1.00 | |
| SO4 | 77.47% | n/a | |
| Oxide Weight | 231.84 | ||
| Formula Weight | 1,029.03 | ||
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| URLs |
http://en.wikipedia.org/wiki/Tungsten_disulfide
Tungsten disulfide at Wikipedia |
| Materials |
Tungsten Trioxide
|