Molybdenum Disulfide

Oxide Analysis Formula Tolerance
MoO3 89.88% 1.00
LOI 10.12%n/a
Oxide Weight 143.94
Formula Weight 160.15

Related Information

Links

Hazards Molybdenum Compounds Toxicology
URLs http://en.wikipedia.org/wiki/Molybdenum_disulfide