Heraeus Schauer Frit K 1325

Alternate Names: Frit K1325

Description: High-sodium low alumina frit

Oxide Analysis Formula Tolerance
CaO 0.05% -
MgO 0.08% -
Na2O 22.58% 0.90
PbO 8.70% 0.10
B2O3 8.93% 0.32
Al2O3 0.21% 0.01
SiO2 59.45% 2.44
Oxide Weight 246.28
Formula Weight 246.28

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.