Mapico 1075A Yellow Iron Oxide

Alternate Names: Pigment Yellow 42

Description: Ferric Oxide Hydrate

Oxide Analysis Formula Tolerance
Fe2O3 87.00% 1.00
H2O 12.00%n/a
Oxide Weight 160.00
Formula Weight 181.82

Notes

Manufacturer using the Martin process.
Typical trace elements ppm: As < 1, Sb < 8, Cd < 1, Cr < 5, Cu < 1, Pb < 3, Hg < 0.1, Ni < 150, Se < .5

Related Information

Links

Materials YLO-1888D Yellow Iron Oxide
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Data

% Passing 325 Mesh Wet .02
Density (Specific Gravity) 4.1
pH for dry powder 6.5