Frit A 1316

Description: Reimbold & Strick lead monosilicate frit

Oxide Analysis Formula Tolerance
SiO2 21.20% 1.00
PbO 78.80% 1.00
Oxide Weight 283.25
Formula Weight 283.25

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Ferro Frit 3377
Materials Lead Monosilicate Frit
A standard frit of 1 molar part of PbO and 1 of SiO2. It melts lower than a lead bisilicate.
URLs http://www.reimbold-und-strick.de/en/index-eng/
Reimbold & Strick website
URLs http://www.reimbold-und-strick.de/images/pdf/keramisch.pdf
Reimbold & Strick Frit chart with chemistry

Data

Co-efficient of Linear Expansion 90 x 10-7 (20-400C)
Frit Softening Point 470C
Glass Transition Temperature 440C