Lead Oxide and Boric Oxide Eutectic

Oxide Analysis Formula Tolerance
PbO 88.00% 1.00
B2O3 12.00% 0.44
Oxide Weight 253.64
Formula Weight 253.64

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 493C