Manganous Oxide and Calcined Kaolin Eutectic

Oxide Analysis Formula Tolerance
MnO 38.90% 2.00
Al2O3 28.00% 1.00
SiO2 33.10% 2.01
Oxide Weight 364.29
Formula Weight 364.29

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

Frit Softening Point 1120C