Magnesia and Calcined Kaolin Eutectic

Oxide Analysis Formula Tolerance
MgO 26.60% 1.00
Al2O3 33.60% 0.50
SiO2 39.80% 1.00
Oxide Weight 151.50
Formula Weight 151.50

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

Frit Softening Point 1330C
By Tony Hansen