Hommel Frit 490

Oxide Analysis Formula Tolerance
Na2O 7.59% 0.30
CaO 14.66% 0.65
MgO 0.79% 0.05
Al2O3 4.31% 0.10
B2O3 16.21% 0.58
SiO2 43.59% 1.80
ZrO2 12.94% 0.26
Oxide Weight 248.15
Formula Weight 248.15

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.5 x 10-6
Frit Melting Range (C) 1550F