Ca Fluoride & Ca Metasilicate Eutectic

Formula: CaF2

Notes

The eutectic mix is CaF2 38.1, CaO 29.8, SiO2 32.1

Related Information

Links

Oxide Analysis Formula Tolerance
Glossary Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures.
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1130C