1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Na & Ca Metasilicate Eutectic

Formula: 3.8Na2SiO3 . CaSiO3

Oxide Analysis Formula Tolerance
SiO2 49.80% 1.00
CaO 9.60% 0.21
Na2O 40.60% 0.79
Oxide Weight 121.07
Formula Weight 121.07

Related Information

Links

Glossary Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures.
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 932C