Alternate Names: Fusion Frit F577
Description: Calcium magnesium zirconium matt frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 1.50% | 0.04 | |
| CaO | 15.50% | 0.45 | |
| MgO | 12.60% | 0.51 | |
| Al2O3 | 3.50% | 0.06 | |
| B2O3 | 6.40% | 0.15 | |
| SiO2 | 55.00% | 1.49 | |
| ZrO2 | 5.50% | 0.07 | |
| Oxide Weight | 163.09 | ||
| Formula Weight | 163.09 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 5.8 x 10-6 |
|---|---|
| Frit Softening Point | 1700F |