Fusion Frit F-359

Alternate Names: Fusion Frit F359

Description: Low expansion flux

Oxide Analysis Formula Tolerance
Na2O 0.10% -
CaO 3.40% 0.13
MgO 16.00% 0.86
Al2O3 19.50% 0.42
SiO2 61.00% 2.21
Oxide Weight 217.75
Formula Weight 217.75

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.0 x 10-6
Frit Softening Point >1900F