Alternate Names: Fusion Frit 294
Description: Calcium Magnesium flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 33.20% | 0.68 | |
| MgO | 11.00% | 0.32 | |
| Al2O3 | 7.20% | 0.08 | |
| SiO2 | 48.60% | 0.94 | |
| Oxide Weight | 115.64 | ||
| Formula Weight | 115.64 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 4GF135E
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.39 x 10-6 |
|---|---|
| Frit Softening Point | 1750F |
| By Tony Hansen Follow me on ![]() | ![]() |