Ferro Frit 4108

Alternate Names: Frit 4508, Frit DA4108, Frit KPM 4108

Description: Low alumina high CaO boro silicate frit

Oxide Analysis Formula Tolerance
CaO 16.68% 0.68
Na2O 8.64% 0.32
Al2O3 3.12% 0.07
B2O3 19.33% 0.64
SiO2 52.23% 1.99
Oxide Weight 229.00
Formula Weight 229.00

Notes

Formerly Frit 4508

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 4144
Materials Ferro Frit 1077
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 583C
Frit Melting Range (C) 1040-1100C
Glass Transition Temperature 618C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy