Description: SOUTH CAROLINA KAOLIN
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
McNamee Kaolin
|
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
Peerless 3 Kaolin
|
| Materials |
Bilt-Cote Kaolin
|
| Materials |
Langford Kaolin
|
| Materials |
Peerless 2 Kaolin
|
| Materials |
PAR Kaolin
|
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| URLs |
https://www.vanderbiltminerals.com/resources/Minerals_and_Chemical_for_Ceramics_and_Refractories_web.pdf
Vanderbilt Minerals for Ceramics Technical Sheet Includes Vansil, Pyrax, Peerless, Dixie, Veegum, Vanzan, Darvan. |
| GE Brightness | 70 |
|---|---|
| % Passing 325 Mesh Wet | 99.8% |
| Moisture Content - Powder | 1% Max |
| Median Particle Size (Microns) | 0.2 microns |